今天給大家進行一番鋼材知識講解,即熱軋帶肋鋼筋檢驗時,到底是要如何檢驗。本文主要分為五點,不知道的趕緊拿小本本記下來了。
Today, I will give you a knowledge of steel, that is, how to test hot-rolled ribbed steel bar. This article is mainly divided into five points, do not know to take a small book to write down.
鋼筋檢驗
Steel bar inspection
進行鋼筋檢驗時,要說的是如何如何進行鋼筋內徑檢驗,方法為:用游標卡尺測量;帶肋鋼筋內徑的測量應該精確到0.1mm。
When inspecting reinforcing bars, the first thing to say is how to inspect the inner diameter of reinforcing bars. The method is to measure the inner diameter of reinforcing bars with vernier calipers and to measure the inner diameter of ribbed bars accurately to 0.1 mm.
對于橫肋高檢驗時,方法為:用游標卡尺測量,帶肋鋼筋橫肋高度高度的測量采用測量同一截面兩側橫肋中心高度平均值的方法,應精確到0.1mm。
For the test of cross rib height, the method is: using vernier caliper to measure the height of cross rib of ribbed steel bar, using the method of measuring the average height of the center of cross rib on both sides of the same section, which should be accurate to 0.1 mm.

對于鋼筋重量偏差的檢測,方法為:用電子秤測量(0—6kg),測量鋼筋重量偏差時,試驗更應從不同根鋼筋上截取,數量不少于5支,每支試驗長度不小于500mm,長度應逐支測量,應準確到1mm,測量試樣總重量時,應精確到不大于總重量1%。
For the detection of the weight deviation of reinforcing steel bar, the method is as follows: when measuring the weight deviation of reinforcing steel bar with electronic scale (0-6kg), the test should be intercepted from different reinforcing steel bars, with a number of no less than 5 bars. The length of each bar should be no less than 500 mm, and the length should be measured one by one, and the total weight of the sample should be measured accurately to no more than 1% of the total weight.
對于鋼筋的表面標志,現場查看登記即可。
For the surface marking of steel bar, check and register on site.
而對于鋼筋的物理、化學性能檢測,還需要取樣送檢。
The physical and chemical properties of steel bars need to be sampled for inspection.
關于鋼筋檢驗的小方法,就介紹到這里了。天翔成也會盡力,為大家帶來更多鋼材方面的小知識!
This is the introduction of the small method of steel bar inspection. Tianxiangcheng will do his best to bring you more knowledge about steel.